Product Description

Alcohol-based coating for sand casting Sand casting with alcohol-based coatings

Performance Features

·This product series exhibits excellent suspension stability, remaining free of caking, sedimentation, and gas evolution during long-term storage and long-distance transportation. It also boasts outstanding anti-sand-sticking performance, easy coating removal and cleanup, and effectively eliminates bubbling and peeling, thereby preventing surface defects in castings.

How to Use :

This product series is supplied in a slurry or paste form. Prior to use, an appropriate amount of alcohol should be added and the mixture thoroughly stirred and diluted to the desired Baumé degree before being introduced into the coating tank for application. Detailed instructions for each specific model are available upon request. It is recommended to use a dedicated dilution and mixing device to dilute the coating and adjust its Baumé degree. Once the coating has been adjusted to the specified Baumé degree, proceed with the application process.

  1. Stir the paint in the container thoroughly using a dedicated mixer or a manual stirrer.
  2. Pour the thoroughly mixed coating into the coating dilution tank or container, start the agitator, and add an appropriate amount of alcohol while stirring. 15-20 After one minute, stop stirring; allow the coating to stand still for another minute, then measure its Baumé degree. Repeat the above procedure until the desired Baumé degree is achieved.
  3. Once the coating’s Baumé degree meets the specified requirements, brushing, dipping, or flow coating may be carried out. For the specific Baumé range and application method, please refer to the detailed product manual.
  4. For brush application, wool brushes or soft-bristle brushes are recommended. For flow coating, specialized flow-coating equipment must be used, and the coating should be applied in a sequential manner; during flow coating, the coating pressure should not be too high to prevent splattering. Whether applying by brushing, dipping, or flow coating, it is essential to ensure uniform coating thickness and to avoid defects such as buildup, runs, and drips. If necessary, use a brush to smooth out any areas of buildup or runs. When more than two coats are required, wait until the temperature of the previous coat has cooled to room temperature before applying the next coat, to avoid applying while the coating is still hot.
  5. Alcohol-based coatings can be ignited and dried, making the process convenient and fast—no oven drying is required, which helps boost production efficiency. Typically, after brushing or flow coating, simply wait a short while. 1-3 Allow the solvent to penetrate and mat the finish for a few minutes before ignition. Continuous brushing or flow coating is also acceptable. 2 — 3 Next time, light it once.
  6. After the second and subsequent coats of alcohol-based coating are applied by brushing, the coating ignites and burns rapidly, posing a risk of burns to the operator; ensure that the face is kept well clear of the top of the mold.
  7. For certain sand cores that are prone to deformation, cracking, or scorching, ignition should be delayed or omitted altogether to allow them to dry naturally.

Common specifications and models:

Sand Mold Coating (Alcohol-Based) Model

Main Aggregate

Scope of Application

Application Method

Sand Mold 300 Series

Zirconium powder

Stainless steel, extra-large cast steel parts

Brush coating, flow coating

Sand Mold Series 307

Corundum

Small and medium-sized cast steel parts

Brush coating, flow coating, and dip coating

Sand Mold Series 309

Mullite composite

Thick Carbon Steel Castings

Brush coating, flow coating

Sand Mold Manganese Steel Series

Magnesia

Wear-resistant cast steel parts

Brushing and spraying

Sand Mold 500 Series

Mullite

Ductile iron and gray iron castings

Brush coating, flow coating, spray coating

Sand Mold 400 Series

Magnesium oxide

For seepage prevention only

Brush coating, flow coating, spray coating

Sand Mold Series 508

Andalusite composite

Gray iron and ductile iron castings

Brush coating, flow coating, spray coating

Sand Mold 800 Series

Mullite composite

Large ductile iron castings

Brush coating, flow coating, spray coating

Storage and Transportation

·Shelf life: 3 month

· Keep away from sources of ignition during storage, transportation, and use.

Packaging

·Barrel-packed 40kg/ Barrel, barrel-packed 30kg/ Barrel and bag packaging 25 kg/ bag

Keywords:

Alcohol-Based Coating for Sand Casting

Previous:

Next:

Application Cases

3f9bc92edfb30aaae773973682a58c54.jpg
58150bc79367df99168fd08251d7a45.jpg
3f9bc92edfb30aaae773973682a58c54.jpg
58150bc79367df99168fd08251d7a45.jpg

Sand-mold wear-resistant parts

79f049cd8ecf9f65033263ef3473435.jpg
307系列.png
0443eb6f0f3d7978b285c2bc0c9470b.jpg
800系列涂料刷涂.png
800系列涂料刷涂2.png
8786607cb6d8d7f45477e1dd7eb89d4.jpg
271318477575b771bc8b9e44a9b51f5.jpg
a5e5779153be9f3763d2542b5e471b5.jpg
机床件500系列.png
砂型铸钢件300涂料.png
砂型铸钢轧罐309系列.png
图片2(1766490163564).png
79f049cd8ecf9f65033263ef3473435.jpg
307系列.png
0443eb6f0f3d7978b285c2bc0c9470b.jpg
800系列涂料刷涂.png
800系列涂料刷涂2.png
8786607cb6d8d7f45477e1dd7eb89d4.jpg
271318477575b771bc8b9e44a9b51f5.jpg
a5e5779153be9f3763d2542b5e471b5.jpg
机床件500系列.png
砂型铸钢件300涂料.png
砂型铸钢轧罐309系列.png
图片2(1766490163564).png

Sand-mold steel casting

a7af4f6f6710df39d3683bd9a4ca59d.jpg
dabbf466f848f79b09553a2b961885f.jpg
a7af4f6f6710df39d3683bd9a4ca59d.jpg
dabbf466f848f79b09553a2b961885f.jpg

Sand-cast aluminum

4ef179c24bdfc964998729abe35137e.jpg
7fb6350b0b06808e8176e7d41c09f03.jpg
8d09dc921194d6f0f9984d4c06dbaf2.jpg
9f24ff54c2004a594171779158c95ed.jpg
25a7f6cfbec822503269703ac4e82d9.jpg
40a272e83a982409d82a16c3c7b0a62.png
50ef31fb00168742e8137036220dd85.jpg
55cbd8d875e49ff52e4b6b91677c31c.jpg
7314ed01c09917f3770fbe6cd511a74.jpg
361618c0536a7c0a8ef5f94ba912624.jpg
400580e16cbba130a1a2d6213fe9db6.jpg
32147380747a037252ff8a343a1234e.jpg
aa112585d32a0389bd18c2705fa6b15.jpg
c0c5d76b6ce1bcbd9d82b65ff3df061.jpg
d5b3c4312e1e207463a58c4f23d790e.jpg
f619b33ff806b39dc426e02df227ff7.jpg
f9941d5056da2eb8c2361c80ead2b5e.jpg
f613870775a9ea867e9d0bb79323b2b.jpg
风电支座800系列.jpg
风电支座800系列1.jpg
风电支座800系列2.jpg
砂型500系列钢锭模铸件.jpg
未抛丸前剥离效果.jpg
4ef179c24bdfc964998729abe35137e.jpg
7fb6350b0b06808e8176e7d41c09f03.jpg
8d09dc921194d6f0f9984d4c06dbaf2.jpg
9f24ff54c2004a594171779158c95ed.jpg
25a7f6cfbec822503269703ac4e82d9.jpg
40a272e83a982409d82a16c3c7b0a62.png
50ef31fb00168742e8137036220dd85.jpg
55cbd8d875e49ff52e4b6b91677c31c.jpg
7314ed01c09917f3770fbe6cd511a74.jpg
361618c0536a7c0a8ef5f94ba912624.jpg
400580e16cbba130a1a2d6213fe9db6.jpg
32147380747a037252ff8a343a1234e.jpg
aa112585d32a0389bd18c2705fa6b15.jpg
c0c5d76b6ce1bcbd9d82b65ff3df061.jpg
d5b3c4312e1e207463a58c4f23d790e.jpg
f619b33ff806b39dc426e02df227ff7.jpg
f9941d5056da2eb8c2361c80ead2b5e.jpg
f613870775a9ea867e9d0bb79323b2b.jpg
风电支座800系列.jpg
风电支座800系列1.jpg
风电支座800系列2.jpg
砂型500系列钢锭模铸件.jpg
未抛丸前剥离效果.jpg

Sand-cast iron

Online Inquiry

If you have any suggestions, please leave us a message or send an email, and we will respond to you within one business day of receiving your email.

Submit